期刊名称:IOP Conference Series: Earth and Environmental Science
印刷版ISSN:1755-1307
电子版ISSN:1755-1315
出版年度:2018
卷号:108
期号:5
页码:052055
DOI:10.1088/1755-1315/108/5/052055
语种:English
出版社:IOP Publishing
摘要:In order to improve the activation effect of deactivation catalysts, calcination of V2O5-WO3-MoO3/TiO2 catalysts were investigated. The experimental results demonstrate that calcination time have an effect for recovering the activity of V2O5-WO3-MoO3/TiO2 catalyst. Calcination not only ensures the better mechanical strength and integrity of the catalyst, but also plays an important role in the denigration activity of the catalyst. However, the particles of the catalyst surface enlarged with the increase of the calcination temperature. The suitable calcination time can improve the denigration efficiency and increase the mechanical strength of the catalyst. In addition, the calcination time mainly affects the formation of MoO3. These findings can provide reference for the activation of SCR-Den Ox catalyst.