摘要:= 50 W and then annealed at 400 °C, a huge saturation field is achieved (over 40 kOe) indicating a very strong PMA. Between the two interfaces of Pt/Co and Co/MgO, the PMA is mainly due to the former in the as-deposited state, but the contribution of the latter increases with the increase in the annealing temperature.